Aluminum is light, it does not rust like steel, and it moves heat away from the weld very quickly. It is also covered in a hard oxide skin that melts at a far higher temperature than the metal under it. Good aluminum welds start long before the arc: with clean metal, the right filler and a joint fitted tight enough that the puddle can bridge it without sagging.
The aluminum parts we weld
Most of our aluminum work is brackets, mounts, covers, small boxes, handles, tabs and light frames for equipment. Product designers send us prototype parts in aluminum sheet and tube, equipment builders send repeat brackets, and maintenance teams bring in covers and mounts that need a new tab or a repaired corner.
We weld aluminum with TIG on alternating current, which breaks up the oxide skin while the arc runs. That lets us control the puddle on thin sheet and wet in both edges of a joint, so the weld looks like a row of even ripples rather than a lump.
Prep is most of the work
Aluminum has to be cleaner than any other metal we weld. Grease, marker, old paint and the oxide skin all come off first: a solvent wipe, then a stainless brush used only on aluminum, then welding soon after, before a new skin forms. Skipping any of these steps shows up as dirty, porous welds.
Because aluminum spreads heat so fast, thin parts can go from not melting to melting through in a moment. We use backing bars, tack often and plan the order of welds so the part stays straight. Thick sections next to thin ones take extra thought, and we talk through those joints when we review your drawing.
Finished aluminum parts can be left as welded, brushed, or sent on to anodizing or powder coat by a shop you choose. If a finish follows, tell us; it changes how we treat the welds.
Parts we often weld
- Brackets, tabs and mounting plates
- Covers, lids and small boxes
- Light frames for equipment and displays
- Handles and fitted edges on sheet parts
- Prototype parts in sheet and tube
- Repairs to cracked aluminum covers and housings